Effect of maleic anhydride content and ethanol dilution on the polymerization of furfuryl alcohol in wood veneer studied by differential scanning calorimetry
Research output: Contribution to journal › Research article › Contributed › peer-review
Contributors
Details
| Original language | English |
|---|---|
| Pages (from-to) | 1064-1075 |
| Number of pages | 12 |
| Journal | BioResources |
| Volume | 8 |
| Issue number | 1 |
| Publication status | Published - 10 Jan 2013 |
| Peer-reviewed | Yes |
External IDs
| Scopus | 84876108371 |
|---|---|
| ORCID | /0000-0002-8854-7726/work/142242046 |
| ORCID | /0000-0001-6999-6182/work/195296663 |