Planar-Biaxial Thermo-mechanical Fatigue Behavior of Nickel-Base Superalloy Inconel 718 Under Proportional Loading
Research output: Contribution to journal › Research article › Contributed › peer-review
Contributors
Abstract
The planar-biaxial thermo-mechanical fatigue behavior of nickel-base superalloy Inconel 718 was studied for selected proportional loading conditions, in particular biaxial strain ratios of 1.0, 0.6, and − 1.0. The cyclic temperature loading with minimum and maximum temperatures of 400 °C and 630 °C and a duration of 250 seconds was either In-Phase or Out-of-Phase to the mechanical axes. Besides the multiaxial tests, uniaxial thermo-mechanical fatigue tests were conducted In-Phase and Out-of-Phase with the same temperature cycle and cycle duration. The performed thermo-mechanical fatigue tests were analyzed regarding the deformation and lifetime behavior and compared with high-temperature isothermal low-cycle fatigue tests from a previous work of the authors. On the side of the lifetime description, a strain- and a stress-based approach were presented. For the planar-biaxial tests, the crack initiation mechanism and crack paths were shown.
Details
| Original language | English |
|---|---|
| Pages (from-to) | 1971–1984 |
| Number of pages | 14 |
| Journal | Metallurgical Transactions A (Physical Metallurgy and Materials Science) |
| Volume | 54 |
| Issue number | 5 |
| Early online date | 25 Nov 2022 |
| Publication status | Published - May 2023 |
| Peer-reviewed | Yes |
External IDs
| Scopus | 85142652083 |
|---|