Hemocompatibility of cellulose phosphate aerogel membranes with potential use in bone tissue engineering

Research output: Contribution to journalResearch articleContributedpeer-review

Contributors

  • Christian B Schimper - , Department of Chemistry, Institute of Chemistry of Renewable Resources, University of Natural Resources and Life Sciences Vienna, Vienna, Austria. (Author)
  • Paul Pachschwöll - , Department of Chemistry, Institute of Chemistry of Renewable Resources, University of Natural Resources and Life Sciences Vienna, Vienna, Austria. (Author)
  • Manfred F Maitz - , Leibniz Institute of Polymer Research Dresden (Author)
  • Carsten Werner - , Leibniz Institute of Polymer Research Dresden (Author)
  • Thomas Rosenau - , Department of Chemistry, Institute of Chemistry of Renewable Resources, University of Natural Resources and Life Sciences Vienna, Vienna, Austria. (Author)
  • Falk Liebner - , Department of Chemistry, Institute of Chemistry of Renewable Resources, University of Natural Resources and Life Sciences Vienna, Vienna, Austria. (Author)

Abstract

Cellulose is an appealing material for tissue engineering. In an attempt to overcome some obstacles with cellulose II cell scaffolding materials related to insufficient biomineralization, lack of micron-size porosity, and deficiency in surface charge, respective solutions have been proposed. These included covalent phosphorylation of different cellulose materials targeting relatively low degrees of substitution (DS 0.18-0.23) and processing these cellulose derivatives into scaffolding materials by a dissolution/coagulation approach employing the hitherto rarely used TBAF/DMSO/H 2O system for cellulose dissolution. Here, we report bioactivity and preliminary hemocompatibility testing of dual-porous cellulose phosphate aerogels (contrasted with the phosphate-free reference) obtained via coagulation (water/ethanol), solvent exchange and scCO 2 drying. Deposition of hydroxyapatite from simulated body fluid (7 days of immersion) revealed good bioactivity (1.5-2.2 mg Ca 2+ per mg scaffold). Incubation of the scCO 2-dried and rehydrated scaffolding materials in heparin anticoagulated human whole blood was conducted to study selected parameters of hemostasis (prothrombin F1+2 fragment, PF4, count of thrombocyte-leukocyte conjugates) and inflammatory response (C5a fragment, leukocyte activation marker CD11b). Adhesion of leukocytes on the surface of the incubated substrates was assessed by scanning electron and fluorescence microscopy (DAPI staining). The results suggest that phosphorylation at low DS does not increase platelet activation. However, a significant increase in platelet activation and thrombin formation was observed after a certain fraction of the negative surface charges had been compensated by Ca 2+ ions. The combination of both phosphorylation and calcification turned out to be a potent means for controlling the inflammatory response, which was close to baseline level for some of the studied samples.

Details

Original languageEnglish
Article number1152577
Pages (from-to)1152577
JournalFrontiers in bioengineering and biotechnology
Volume11
Publication statusPublished - 2023
Peer-reviewedYes
Externally publishedYes

External IDs

PubMedCentral PMC10154571
Scopus 85159779714
ORCID /0000-0003-0189-3448/work/173985684

Keywords