Analysis of the pore size distribution and fiber saturation point of native and thermally modified wood using differential scanning calorimetry

Research output: Contribution to journal › Research article › Contributed › peer-review

Details

Original languageEnglish
Pages (from-to)177–193
Number of pages17
JournalWood Science and Technology
Volume48
Publication statusPublished - 2014
Peer-reviewedYes

External IDs

researchoutputwizard legacy.publication#57928
Scopus 84893711463
ORCID /0000-0001-6999-6182/work/195296657

Keywords

Keywords

  • Analyse, Porengrößenverteilung, Fasersättigungspunkt, thermische Modifizierung, Holz, DSC