Structuring large area WS2 layers grown by atomic layer deposition

Publikation: Beitrag in Fachzeitschrift › Forschungsartikel › Beigetragen › Begutachtung

Beitragende

  • Leon Doman - , Fraunhofer-Institut für Mikroelektronische Schaltungen und Systeme (Autor:in)
  • Nils Boysen - , Fraunhofer-Institut für Mikroelektronische Schaltungen und Systeme (Autor:in)
  • Thomas Gemming - , Leibniz-Institut für Festkörper- und Werkstoffforschung Dresden (Autor:in)
  • Haowen Shi - , Fraunhofer-Institut für Mikroelektronische Schaltungen und Systeme (Autor:in)
  • Anjana Devi - , Professur für Materialchemie (gB/IFW), Fraunhofer-Institut für Mikroelektronische Schaltungen und Systeme, Leibniz-Institut für Festkörper- und Werkstoffforschung Dresden (Autor:in)

Abstract

The large-scale deposition and integration of 2D materials on 200 mm wafers for emerging microelectronic applications are highly challenging. Throughout the processing, significant issues in controlling material growth and patterning must be addressed. Therefore, this study introduces a new approach for bottom-up growth and subsequent patterning of ultrathin 2D WS2 layers on 200 mm wafers. To achieve this, atomic layer deposition (ALD) was used to grow WS2 thin films directly on 200 mm wafers, which were then patterned by photolithography and ion-beam etching. To prevent degradation and delamination of the WS2 layer during patterning, an in situ Al2O3 ALD capping layer is employed. Even after treatment in boiling de-ionized water, which porosifies the Al2O3 as needed for sensing applications, the WS2 and underlying features remain intact. To investigate the effects of patterning and capping processes in detail, Raman spectroscopy, scanning electron microscopy, and transmission electron microscopy were used. The detailed analysis shows that the proposed strategies enable patterning of WS2 layers on 200 mm wafers using Al2O3 capping layers. Electrical measurements of the WS2 patterned on interdigitated electrodes show a linear current response and an average resistance of 0.4 ± 0.26 MΩ across the 200 mm wafer. Overall, our findings indicate a promising step toward the scalable integration of WS2 into various micro- and nanosystems, especially sensors, and support future scaling of these processes.

Details

OriginalspracheEnglisch
Aufsatznummer032203
FachzeitschriftJournal of Vacuum Science and Technology A: Vacuum, Surfaces and Films
Jahrgang44
Ausgabenummer3
PublikationsstatusVeröffentlicht - 1 Mai 2026
Peer-Review-StatusJa