Assessing the Environmental Impact of Atomic Layer Deposition (ALD) Processes and Pathways to Lower It
Publikation: Beitrag in Fachzeitschrift › Übersichtsartikel (Review) › Beigetragen › Begutachtung
Beitragende
Abstract
Due to concerns on resources depletion, climate change, and overall pollution, the quest toward more sustainable processes is becoming crucial. Atomic layer deposition (ALD) is a versatile technology, allowing for the precise coating of challenging substrates with a nanometer control over thickness. Due to its unique ability to nanoengineer interfaces and surfaces, ALD is widely used in many applications. Although the ALD technique offers the potential to tackle environmental challenges, in particular, considerations regarding the sustainability of renewable energy devices urge for greater efficiency and lower carbon footprint. Indeed, the process itself has currently a consequential impact on the environment, which should ideally be reduced as the technique is implemented in a wider range of products and applications. This paper reviews the studies carried out on the assessment of the environmental impact of ALD and summarizes the main results reported in the literature. Next, the principles of green chemistry are discussed, considering the specificities of the ALD process. This work also suggests future pathways to reduce the ALD environmental impact; in particular, the optimization of the reactor and processing parameters, the use of high throughput processes such as spatial ALD (SALD), and the chemical design of greener precursors are proposed as efficient routes to improve ALD sustainability.
Details
| Originalsprache | Englisch |
|---|---|
| Seiten (von - bis) | 274-298 |
| Seitenumfang | 25 |
| Fachzeitschrift | ACS Materials Au |
| Jahrgang | 3 |
| Ausgabenummer | 4 |
| Publikationsstatus | Veröffentlicht - 12 Juli 2023 |
| Peer-Review-Status | Ja |
| Extern publiziert | Ja |
Externe IDs
| PubMed | 38090128 |
|---|
Schlagworte
Ziele für nachhaltige Entwicklung
- SDG 7 – Erschwingliche und saubere Energie - atomic layer deposition, green chemistry, precursors, spatial ALD, synthesis
- SDG 13 – Klimaschutzmaßnahmen - atomic layer deposition, green chemistry, precursors, spatial ALD, synthesis
ASJC Scopus Sachgebiete
- Elektronische, optische und magnetische Materialien - atomic layer deposition, green chemistry, precursors, spatial ALD, synthesis
- Biomaterialien - atomic layer deposition, green chemistry, precursors, spatial ALD, synthesis
- Polymere und Kunststoffe - atomic layer deposition, green chemistry, precursors, spatial ALD, synthesis
- Werkstoffchemie - atomic layer deposition, green chemistry, precursors, spatial ALD, synthesis
Schlagwörter
- atomic layer deposition, green chemistry, precursors, spatial ALD, synthesis